Customization: | Available |
---|---|
Type: | Steel Plate |
Standard: | ASTM, AISI, GB, DIN |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
The following material properties are ASTM specifications and will be confirmed on the Mill Test Report.
GRADE | YIELD POINT (KSI) | TENSILE STRENGTH (KSI) | MIN. 8" ELONGATION % |
60 | 60 | 75 | 16 |
65 | 65 | 80 | 15 |
The following composition properties are ASTM specifications for the A871 specification. Grades 60 and 65 can be produced with three types of chemical compositions.
TYPE I | |
CARBON | 0.19% MAX |
MANGANESE | 0.80-1.35% |
PHOSPHORUS | 0.030% MAX |
SULFUR | 0.030% MAX |
SILICON | 0.30-0.65% |
NICKEL | 0.40% MAX |
CHROMIUM | 0.40-0.70% |
COPPER | 0.25-0.40% |
VANADIUM | 0.02-0.10% |
TYPE II | |
CARBON | 0.20% MAX |
MANGANESE | 0.75-1.35% |
PHOSPHORUS | 0.030% MAX |
SULFUR | 0.030% MAX |
SILICON | 0.15-0.50% |
NICKEL | 0.50% MAX |
CHROMIUM | 0.40-0.70% |
COPPER | 0.20-0.40% |
VANADIUM | 0.01-0.10% |
TYPE IV | |
CARBON | 0.17% MAX |
MANGANESE | 0.50-1.20% |
PHOSPHORUS | 0.030% MAX |
SULFUR | 0.030% MAX |
SILICON | 0.25-0.50% |
NICKEL | 0.40% MAX |
CHROMIUM | 0.40-0.70% |
MOLYBDENUM | 0.10% MAX |
COPPER | 0.30-0.50% |
COLUMBIUM | 0.005-0.05% |