Customization: | Available |
---|---|
After-sales Service: | Change/Return |
Warranty: | 1 Year |
Still deciding? Get samples of US$ 50/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
JIS G3461 Grade STB 510 Carbon Steel Seamless Tubes are also known as mild steel pipes and tubes.JIS G3461 Grade STB 510 Tubes are low-cost Low Carbon Steel Tubes with max 025 % carbon content with combination of 100-150 % manganese easy to form and shape .These pipes are manufactured as per JIS Specification and commercially referred as cs pipes or ms pipes.Low Carbon Steel Pipes are not as hard as hig carbon steel pipes,Though carburizing can increase its surface hardness.
Chemical Composition
The tube shall be tested in accordance with 9.1 and the resulting ladle analysis values shall conform to Table 2.
Table 2 Chemical Composition
Standard | Grade | Chemical Composition Limits (%) | ||||
C | Si | Mn | P | S | ||
JIS G3461 | STB 340 | ≤ 0.18 | ≤ 0.3 | 0.30-0.60 | ≤ 0.035 | ≤ 0.035 |
STB 410 | ≤ 0.32 | ≤ 0.35 | 0.30-0.80 | ≤ 0.035 | ≤ 0.035 | |
STB 510 | ≤ 0.25 | ≤ 0.35 | 1.00-1.50 | ≤ 0.035 | ≤ 0.035 |
Grade | Tensile Property (N/mm2) | Yield Point or Yield Strength (N/mm2) | Rockwell hardness HRB | Elongation (%) | ||
OD ≥20 mm | 10 mm ≤OD <20 mm | OD <10 mm | ||||
NO. 11 Sample; NO. 12 Sample | NO. 11 Sample | NO. 11 Sample | ||||
Longitudinal | Transverse | Transverse | ||||
STB 340 | ≥ 340 | ≥ 175 | 77 max. | ≥ 35 | ≥ 30 | ≥ 27 |
STB 410 | ≥ 410 | ≥ 255 | 79 max. | ≥ 25 | ≥ 20 | ≥ 17 |
STB 510 | ≥ 510 | ≥ 295 | 92 max. | ≥ 25 | ≥ 20 | ≥ 17 |
Grade | Heat treatment | ||||
Hot finished seamless steel tube | Cold finished seamless steel tube | Electric resistance welded steel tube other than hot finished or cold finished steel tube | Finished electric resistance welded steel tube | Fold finished electric resistance welded steel tube | |
STB 340 | As manufactured, as required, low temperature annealing or normalizing may be performed. | Low temperature annealing,normalizing or full annealing. |
Normalizing | As manufactured. However, as required, low temperature annealing or normalizing may be performed | Normalizing |
STB 410 | As manufactured. However, as required, low temperature annealing or normalizing may be performed. | Low temperature annealing, normalizing or full annealing. |
Normalizing | Low temperature annealing | |
STB 510 | Normalizing |
Symbol of class | Rockwell hardness HRB (Mean value of three points) |
STB 340 STB 410 STB 510 |
77 max. 79 max. 92 max. |