• ASTM A333 Alloy Seamless Steel Pipes
  • ASTM A333 Alloy Seamless Steel Pipes
  • ASTM A333 Alloy Seamless Steel Pipes
  • ASTM A333 Alloy Seamless Steel Pipes
  • ASTM A333 Alloy Seamless Steel Pipes
  • ASTM A333 Alloy Seamless Steel Pipes

ASTM A333 Alloy Seamless Steel Pipes

Type: Seamless
Technique: Cold Drawn
Material: Alloy Steel
Surface Treatment: Varnish,Black Painting,Oild
Usage: Pipeline Transport, Chemical Industry
Section Shape: Round
Samples:
US$ 10/Piece 1 Piece(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2011

Suppliers with verified business licenses

Guangdong, China
High Repeat Buyers Choice
More than 50% of buyers repeatedly choose the supplier
Years of Export Experience
The export experience of the supplier is more than 10 years
Experienced Team
The supplier has 10 foreign trading staff(s) and 7 staff(s) with over 6 years of overseas trading experience
Exhibition Experience
The supplier had participated in offline trade shows, you can check the Audit Report for more information
to see all verified strength labels (18)

Basic Info.

Model NO.
KM-20200716
Od
19.05mm~219.1mm
Wt
2.0mm~15mm
Materials
Gr.1,Gr.2,Gr.3,Gr.4,Gr.5,Gr.6,Gr.7gr.8,Gr.9,etc
Surface
Black Painted Oilded
Delivery Condition
Normalized
Technique Method
Cold Rolled or Cold Drawing
Transport Package
in Bundle or Customer′s Requirement
Specification
19.05mm~219.1mm
Trademark
Kingmetal
Origin
China
HS Code
73045990
Production Capacity
500 Tons Per Month

Product Description

ASTM A333 Alloy Seamless Steel Pipes

Outer Dimensions: 19.05mm~219.1mm
Wall Thickness: 2.0mm~15 mm
Length: Max 16000mm
 

1. ASTM A333 Chemical Composition Requirements

Chemical Composition of ASTM A333
Element Grade 1, % Grade 3, % Grade 4, % Grade 6, % Grade 7, % Grade 8, % Grade 9, % Grade 10, % Grade 11, %
C 0.30 0.19 0.12 0.30 0.19 0.13 0.20 0.20 0.10
Mn 0.40-1.06 0.31-0.64 0.50-1.05 0.29-1.06 0.90 0.90 0.40-1.06 1.15-1.50 0.60
P 0.025 0.025 0.025 0.025 0.025 0.025 0.025 0.035 0.025
S 0.025 0.025 0.025 0.025 0.025 0.025 0.025 0.015 0.025
Si ... 0.18-0.37 0.08-0.37 0.10 min 0.13-0.32 0.13-0.32 ... 0.10-0.35 0.35
Ni ... 3.18-3.82 0.47-0.98 0.40 2.03-2.57 8.40-9.60 1.60-2.24 0.25 35.0-37.0
Cr ... ... 0.44-1.01 0.30 ... ... ... 0.15 0.50
Cu ... ... 0.40-0.75 0.40 ... ... 0.75-1.25 0.15 ...
Al ... ... 0.04-0.30 ... ... ... ... 0.06 ...
V ... ... ... 0.08 ... ... ... 0.12 ...
Cb ... ... ... 0.02 ... ... ... 0.05 ...
Mo ... ... ... 0.12 ... ... ... 0.05 0.50
Co ... ... ... ... ... ... ... ... 0.50
*For Grade 1 and 6, each reduction of 0.01% C below 0.30%, an increase of 0.05 % Mn above 1.06 % would be permitted to a max. of 1.35%.
*For Grade 6, the limit for columbium may be increased up to 0.05 % on heat analysis and 0.06 % on product analysis.
*Generally, the carbon equivalent C.E = [C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15] shall not exceed 0.43% by heat analysis.

2. ASTM A333 Mechanical Properties

ASTM A333 Tensile Strength, min. Yield Strength, min. Elongation %, min.
Grade psi MPa psi MPa Longitudinal Transverse
Grade 1 55 000 380 30 000 205 35 25
Grade 3 65 000 450 35 000 240 30 20
Grade 4 60 000 415 35 000 240 30 16.5
Grade 6 60 000 415 35 000 240 30 16.5
Grade 7 65 000 450 35 000 240 30 22
Grade 8 100 000 690 75 000 515 22 ...
Grade 9 63 000 435 46 000 315 28 ...
Grade 10 80 000 550 65 000 450 22 ...
Grade 11 65 000 450 35 000 240 18 ...
*The elongation values are furnished on the basis of standard round  2 inch or 50 mm(or 4D) specimens.
*Elongation of Grade 11 is for all walls and small sizes tested in full section.

3.  Charpy V-notch Impact Tests

Impact Requirements for Grades 1, 3, 4, 6, 7, 9, 10, and 11
Size of Specimen *A *B
mm ft·lbf J ft·lbf J
10 by 10 13 18 10 14
10 by 7.5 10 14 8 11
10 by 6.67 9 12 7 9
10 by 5 7 9 5 7
10 by 3.33 5 7 3 4
10 by 2.5 4 5 3 4
*A denotes minimum average notched bar impact value of each set of three specimens.
*B denotes minimum notched bar impact value of one specimen only of a set.
Minimum Impact Test Temperature of ASTM A333
Grade °F °C
1 -50 -45
3 -150 -100
4 -150 -100
6 -50 -45
7 -100 -75
8 -320 -195
9 -100 -75
10 -75 -60
11 -320 -195
* Impact tests specified for temperatures lower than 70 °F [20 °C] should be made with precautions.