Customization: | Available |
---|---|
Type: | Seamless |
Material: | Stainless Steel |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
STANDARD | WERKSTOFF NR. | UNS | JIS | AFNOR | BS | KS | EN |
SS 904L | 1.4539 | N08904 | SUS 890L | Z2 NCDU 25-20 | 904S13 | STS 317J5L | X1NiCrMoCu25-20-5 |
Production according to national and international standards (e.g. ASME, ASTM, API, EN, DNV, etc.)
Grade | C | Mn | Si | P | S | Cr | MO | Ni | CU | |
904L | Min | - | - | - | - | - | 19.0 | 4.00 | 23.00 | 1.00 |
max | 0.20 | 2.00 | 1.00 | 0.045 | 0.035 | 23.0 | 5.00 | 28.00 | 2.00 |
Mechanical properties
Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
Rockwell B (HRB) | Brinell (HB) | ||||
904L | 490 | 220 | 35 | 70-90 typical | - |
Rockwell Hardness value range is typical only; other values are specified limits. |
Physical propertie
Grade |
Density (kg/m3) |
Elastic Modulus (GPa) |
Mean Co-eff of Thermal Expansion (µm/m/°C) | Thermal Conductivity (W/m.K) |
Specific Heat 0-100°C (J/kg.K) |
Elec Resistivity (nΩ.m) |
|||
0-100°C | 0-315°C | 0-538°C | At 20°C | At 500°C | |||||
904L | 8000 | 200 | 15 | - | - | 13 | - | 500 | 850 |
Grade specifications
Grade | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
BS | En | No | Name | ||||
904L | N08904 | 904S13 | - | 1.4539 | X1NiCrMoCuN25-20-5 | 2562 | - |
These comparisons are approximate only. The list is intended as a comparison of functionally similar materials not as a schedule of contractual equivalents. If exact equivalents are needed original specifications must be consulted. |