UNS S32750 Properties
Chemical Analysis (% max or range).
C | Mn | P | S | Si | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
0.03 | 1.20 | 0.035 | 0.02 | 0.80 | 24.0 - 26.0 | 6.0 - 8.0 | 3.0 - 5.0 | 0.24 - 0.32 |
Mechanical properties
Tensile | Yield | Elongation | Hardness |
---|---|---|---|
MPa min | MPa min | % min | Brinell max |
795 | 550 | 15.25% | 310 |